Table 2. Photogenerated Currents of the Multilayer Composites and Increases in Their Value Compared to Bare TiO2a.
method | LSV (at ∼0.8 V) |
CA (at ∼80 s, 1 V) |
||||
---|---|---|---|---|---|---|
sample | 1L | 2L | 3L | 1L | 2L | 3L |
photocurrent (μA) | 3.062 | 3.567 | 3.635 | 2.664 | 3.025 | 3.054 |
photocurrent increase vs TiO2 (%) | 39.95 | 63.03 | 66.13 | 42.08 | 61.33 | 62.88 |
1L, 2L, 3L—PDA/TiO2 one layer, two layer, and three layer composites, respectively.