Skip to main content
. 2024 Mar 4;14(11):7490–7498. doi: 10.1039/d3ra08967c

Saturation magnetization (Ms), coercivity (Hc), of different as-prepared Co–C alloys and hcp Co.

Sample PT condition M s (emu g−1) H c (Oe) Ref.
hcp Co 175.25 122.15 40
fcc Co 8 66
Co–C alloys 3 GPa, 1300 °C 93.82 (2) 45.66 (4) This work
5 GPa, 1300 °C 93.71 (2) 74.80 (2) This work