Summary of the key characterisation results for the PDEVP@AuNPs and their precursors (citrate@AuNPs and dopazide@AuNPs), as well as for the two control experiments (test (i) and test (ii)).

Sample D TEM [nm] D h [nm] ζ-Potential [mV]
Citrate@AuNPs 25.8 ± 7.1 32 ± 0.9 −38.2 ± 2.5
Dopazide@AuNPs 27.8 ± 7.5 48 ± 0.5 −31.5 ± 1.0
PDEVP@AuNPs 25.9 ± 4.1 78.8 ± 1.5 +4.9 ± 0.4
Test (i) (polymer w/o alkyne) 122.9 ± 9.8 +3.1 ± 0.3
Test (ii) (no cat.) 70.0 ± 2.0 −6.7 ± 0.4