Skip to main content
. 2024 Feb 27;9(10):12046–12059. doi: 10.1021/acsomega.3c09926

Table 2. ICP-MS Quantitative Analysis of Zr Content in CeO2 Powders after the Longest Exposure (8 h) to HE Milling Conditions.

sample Zr (wt %) Zr/(Ce+Zr)a (%)
HSA-HE-8h 0.12 0.23
MSA-HE-8h 0.53 0.99
LSA-HE-8h 0.61 1.14
a

Calculated as the atomic ratio between Zr and total Zr+Ce cations.