Skip to main content
. 2024 Feb 29;124(5):2281–2326. doi: 10.1021/acs.chemrev.3c00532

Figure 13.

Figure 13

(a) Variation of the lattice parameters with temperature of the MA0.8GA0.2PbI3 system as determined from the XRD data. (b–d) Temperature dependence of the real part of the complex dielectric permittivity ε′ of the MA1–xGAxPbI3 pellet samples at frequencies between 10 kHz and 1 MHz. Reprinted with permission from ref (355). Copyright 2022 Royal Society of Chemistry.