Fig. 2.

Fig. 2

Changes in mass (A) and compressive strength (B) of the bioceramic scaffolds after immersion in Tris buffers for 0–6 weeks (n = 3). Changes in the release of Ca (C), Si (D), Mg (E), and Na (F) ions in Tris buffer during the immersion test (results plotted as mean ± SD, n = 3).