Table 2.
Sample | Draw Ratio (dr) | Temperature, °C | Spindle Speed, min−1 × 103 | |
---|---|---|---|---|
Goted | Plate | |||
Base fibers | 3.35 | 70 | 120 | 6800 |
Modified fibers with 12% wt. TEC | 2.80 | 60 | 110 | 7100 |
Modified fibers with 5% and 7% wt. of TEC | 3.28 | 70 | 120 | 6600 |
2.80 | 70 | 120 | 6848 | |
Modified fibers with 5% and 7% wt. of ADO | 3.28 | 70 | 120 | 6600 |
2.80 | 70 | 120 | 6848 |