CuO (0.1 g/ml) |
Methylene blue, 0.0022 g/l |
Dip-coating (glass Substrate) |
82 |
180 |
Visible light |
Current study |
CuO NWs |
Methylene blue, 0.0012 g/l |
Porous CuO nanowire (NW) matrix |
34 |
180 |
Visible light |
62 |
CuO@TiO2-300 |
Methylene blue, 0.0012 g/l |
ALD process was performed on CuO NW |
42 |
180 |
Visible light |
62 |
CuO/ZnO (Simple A) |
Methylene blue, 0.005 g/l |
Spin-coating with Glass Substrate |
44 |
120 |
Xe lamp of 150 W |
63 |
Cu2O |
Methylene blue, 0.005 g/l |
Spray pyrolysis growth technique |
60 |
120 |
solar simulator (Dayan) 100 mW/cm2
|
64 |
CuO |
Methylene blue, 0.003 g/l |
Spraying (glass Substrate) |
74 |
360 |
Visible light |
65 |
CuO-ZnO (1:3) |
Methylene blue, 0.003 g/l |
Spraying (glass Substrate) |
85 |
360 |
Visible light |
65 |
Cu:Co (70:30) |
Methylene blue, 0.003 g/l |
Dip-coating (glass Substrate) |
78 |
240 |
Visible light |
7 |
CuO |
Rhodamine-b, 0.01 g/l |
Sputtering and thermal annealing (glass Substrate) |
56 |
120 |
250W Xenon lamp |
66 |