Skip to main content
. 2024 Feb 16;57(Pt 2):248–257. doi: 10.1107/S1600576724000554

Figure 8.

Figure 8

Rietveld refinement of (a) NdGaD0.9 and (b) NdGaD1.6 from the 90° detector bank 3 at 20 K with R wp = 6.00 and 6.03%, respectively. The bottom rows of Bragg reflections correspond to a secondary phase, TaGaO4 (0.5%).