Electrochemical stability of Co-POM-TMOS electrode

(A) Constant Potential Electrolysis (CPE) recorded at 1.6 V for Co-POM-TMOS sol-gel electrode.

(B) Comparison of LSVs of Co-POM-TMOS before and after continuous reusing for electrochemical study for 30 days, scan rate: 50 mV/s, 0.2 M NaClO4, pH 2.