Skip to main content
. 2024 Feb 7;11(14):2309254. doi: 10.1002/advs.202309254

Figure 3.

Figure 3

a,b) SEM images and c) COMSOL simulation of the Li/Li13Sn5@CC electrode after Li‐fully stripping. d,e) SEM images and f) COMSOL simulation of replating 5 mAh cm−2 Li on the Li13Sn5@CC electrode. g,h) SEM images and i) COMSOL simulation of replating 20 mAh cm−2 Li on the Li13Sn5@CC electrode. Schematic illustration of the j) Li stripping and k) replating processes of the Li13Sn5@CC electrode.