Summary of characteristics identified by FT-ICR MS analysis of degraded (laccase-treated) and non-degraded (negative control) lignin. Standard deviation is shown in brackets and all 13C-containing ions are excluded.

Treatment Timepoint (hours) Average no. of assigned ions Double bond equivalents (DBE) C H O M w (Da) O/C ratio H/C ratio
Negative 0 4005 15.4 (10.2) 32.3 (14.3) 35.7 (16.9) 10.5 (5.4) 606.4 (229.0) 0.37 (0.22) 1.15 (0.37)
2 3916 15.3 (10.0) 31.3 (13.8) 34.0 (15.7) 10.5 (5.3) 593.6 (220.0) 0.38 (0.22) 1.13 (0.37)
24 3933 15.4 (10.2) 31.7 (14.1) 34.5 (16.7) 10.6 (5.4) 599.2 (225.5) 0.38 (0.22) 1.14 (0.38)
Laccase-treated 0 4057 14.9 (10.1) 31.6 (14.1) 35.3 (17.2) 10.5 (5.4) 597.2 (226.0) 0.38 (0.22) 1.16 (0.38)
2 3716 14.7 (9.5) 30.2 (13.3) 33.0 (16.5) 10.5 (5.4) 579.6 (215.3) 0.39 (0.23) 1.13 (0.38)
24 3081 13.7 (9.7) 27.5 (11.7) 29.5 (15.5) 10.2 (5.3) 538.6 (191.7) 0.42 (0.24) 1.13 (0.42)