Binding energy and full width at half maximum (FWHM) of XPS peaks used for deconvolution.

Constituents 654SMO C276
Binding Energy (eV) FWHM (eV) Binding Energy (eV) FWHM (eV)
Fe 706.7 1.05 706.9 1.5
FeO 707.9 1.86 - -
Fe2O3 709.7 1.86 - -
FeOOH 711.9 2.25 712.1 3.06
Cr 573.8 1.41 573.9 1.77
Cr2O3 576.1 2.28 576.3 2.09
Cr(OH)3 577.3 2.61 577.5 2.13
Ni 852.6 1 852.7 1.07
NiO 853.6 1.34 853.6 0.85
Mo 3d5/2 227.3 0.63 227.6 0.75
Mo4+ 3d5/2 228.5 1.96 228.4 1.3
Mo 3d3/2 230.6 1.75 230.7 1.03
Mo6+ 3d5/2 232.1 1.76 232.2 1.84
Mo4+ 3d3/2 233.3 1.58 233.8 1.31
Mo6+ 3d3/2 235.1 1.92 235.2 2.09
O2− 530.1 0.58 530.3 1.39
OH 531.5 1 531.6 1.68
H2O 532.9 0.37 532.8 1.82
Mo6+ 3p3/2 400.0 1.58
Mo4+ 3p3/2 397.7 0.92
Nitride 398.4 0.78 - -
 NH4+ 399.0 0.93 - -