Figure 5

Comparison of hysteresis error at 102 and 103 Hz of CuO ceramic with many giant dielectric oxides: CCTO1, CCTO2, and CCTO3 are CaCu3Ti4O12 sintered 1100, 1050, and 1020 °C, respectively; MgCCTO is Mg–doped CCTO; NNTO is Na + Nb co–doped TiO2; INTO is In + Nb co–doped TiO2; and NSTCTO is (Na1/3Sr1/3Tb1/3)Cu3Ti4O12.