Table 7. Optimized Reaction Conditions from DoE to Prepare Epoxidized Butyl Rubber at 1 h Reaction Rime.
| run | equiv of Oxone | equiv of NaHCO3 | equiv of acetone | % of epoxide at 60 min | % of epoxide at 60 min |
|---|---|---|---|---|---|
| 1 | 1.25 | 6.5 | 18.0 | 14 | 10 |
| 2 | 1.25 | 6.5 | 47.9 | 23 | |
| 3 | 1.25 | 6.5 | 56.2 | 30 | 29 |
| 4 | 1.25 | 6.5 | 64.3 | 40 | |
| 5 | 1.25 | 6.5 | 71.7 | 50 | |
| 6 | 1.88 | 6.5 | 72.0 | 59 | 55 |