Skip to main content
. 2024 May 8;15:3846. doi: 10.1038/s41467-024-47674-x

Fig. 4. The photographs of Ln3+-manipulated RTP materials.

Fig. 4

a The photographs of 4TPYBOH@PVA–Eu (left) and 4TPYBOH@PVA–Tb (right) RTP films that were prepared by being soaked in different Ln3+ concentrations (0.1–20 mg/mL) taken under and after removing the 254 nm UV irradiation. b The photographs of bimetallic Eu3+ and Tb3+-manipulated RTP materials with the increase of the ratio of Tb3+ taken under and after removing the 254 nm UV irradiation, the total Ln3+ concentration is 1 mg/mL.