Cycles of fatigue failure/fatigue lifetime (in years) of the five experimental models

Crown Implant Abutment Screw
Precrystallized ZLS model 5.00/14.29 4.25/12.15 2.89/8.26 1.00/2.87
Crystallized ZLS model 5.00/14.29 1.44/4.13 8.99/25.69 1.00/2.87
PICN model 5.00/14.29 1.42/4.06 2.37/6.76 3.60/10.30
LD model 5.00/14.29 9.77/27.91 5.04/14.39 3.60/10.29
PEEK model 7.07/20.19 1.01/2.90 2.97/8.47 3.61/10.31