Skip to main content
. 2024 May 20;17(10):2464. doi: 10.3390/ma17102464

Figure 8.

Figure 8

The glass fiber-reinforced epoxy composite functionalized with Diels–Alder undergoes fabrication (top left). The woven glass fiber fabrics are separated until halfway into the specimen ((bottom left) and microscopic image). Subsequently, half of the damaged area is healed using a hot press (right) [102] (The figure is available in Open Access).