Skip to main content
. 2024 May 23;10(11):e31720. doi: 10.1016/j.heliyon.2024.e31720

Table 7.

FRP and steel tendon properties.

Characteristics CFRP [[132], [133], [134], [135], [136], [137], [138], [139], [140], [141], [142], [143], [144], [145], [146], [147], [148], [149], [150], [151], [152], [153], [154], [155], [156],[158], [159], [160], [161],200] GFRP [5,31,168] AFRP [7,8,12,13,25,121,169,172] BFRP [3,57,[173], [174], [175],[177], [178], [179], [180], [181], [182]] Steel Tendons [58,76–120,[201], [202], [203], [204], [205]]
Elastic Modulus (GPa) 80–509 30–70 50–131 38–70 180–210
Ultimate Strain (%) 0.013–0.021 0.012–0.037 0.015–0.037 0.024–0.032 0.027–0.129
Longitudinal thermal expansion coefficient (x10 -6/°C) −9 to 0.68 6 to 10 −6 to −2 18 to 26 11 to 13
Poisson's Ratio 0.22–0.38 0.22 0.38 0.2 0.2–0.3