Table 3.
Material | Elongation | Young’s Modulus |
---|---|---|
PANI/PDMS based electrodes [33] | 308% | 75.312 MPa |
TiO2/PDMS based implantable electrode [17] | 293% | 32.9 kPa |
Silk fibroin/Ti3C2 film-based sensor for wearable pressure and electrical signal sensing [36] | — | 1.22 MPa |
Self-healing MXene/PDMS wearable biosensor [37] | 181% | — |
Composition 1 [this work] | 139 ± 11% | 2.61 ± 0.39 MPa |
Composition 2 [this work] | 144 ± 13% | 2.18 ± 0.31 MPa |