Table 7. Composition of Polymeric Compounds in GHR and Hydrochar at 180 and 200 °C.

  celullose hemicelullose lignin-O lignin-C lignin-H
GHR 0.36 0.24 0.11 0.08 0.21
H-180–7.5 0.25 0.16 0.22 0.12 0.25
H-200–5 0.19 0.13 0.32 0.13 0.22
H-200–10 0.17 0.12 0.53 0.14 0.04