Table 1. Surface Area, Pore Volume, and Pore Diameter of Graphene Oxide before and after CO2 Absorption.
| type | surface area SBET | pore volume | pore diameter |
|---|---|---|---|
| GO | 240.776 m2/g | 0.075 cc/g | 3.406 nm |
| recovered GO | 31.946 m2/g | 0.051 cm3/g | 1.941 nm |
| type | surface area SBET | pore volume | pore diameter |
|---|---|---|---|
| GO | 240.776 m2/g | 0.075 cc/g | 3.406 nm |
| recovered GO | 31.946 m2/g | 0.051 cm3/g | 1.941 nm |