Skip to main content
. 2024 Jun 6;9(24):26582–26595. doi: 10.1021/acsomega.4c03232

Figure 10.

Figure 10

SEM images of the (a) RC/CNT/0.3FeS2/PPy-60 (×500) and (b) RC/CNT/0.3FeS2/PPy-60 (×20,000) electrodes after the 10,000 cycles test.