Skip to main content
. Author manuscript; available in PMC: 2025 Jun 1.
Published in final edited form as: Small. 2024 Jan 21;20(26):e2305684. doi: 10.1002/smll.202305684

Table 1.

Hydrodynamic diameters of PSNPs and the observed increase in size upon interaction with GB3 and R2ab.

Bare PSNPs 50 nm 100 nm 200 nm
Hydrodynamic diameter [nm] 47 ± 4 95 ± 3 165 ± 13
Polydispersity [%] 10 ± 2 20 ± 1 23 ± 2
GB3-Coated PSNPs
Δ Hydrodynamic diameter [nm] 42 ± 2 19 ± 1 4 ± 1
Polydispersity [%] 19 ± 5 26 ± 3 25 ± 8
R2ab-Coated PSNPs
Δ Hydrodynamic diameter [nm] 1989 ± 12 1860 ± 50 2630 ± 60
Polydispersity [%] 80 ± 20 63 ± 15 66 ± 16