In vitro corrosion analysis of the three DFT wires with Wire A, Wire B and Wire C filaments after corrosion over 1, 3, and 7 days. The upper three rows of images are taken with optical microscopy and lower three rows of images are taken with SEM-BSE. Scale bar is 50 μm.