Skip to main content
. 2024 Jun 21;17(13):3057. doi: 10.3390/ma17133057

Figure 6.

Figure 6

SEM micrographs with secondary electron detector wear tracks for Q&T DIN 16MnCr5 steel (a,b) with 6 N load, (c,d) with 4 N load, and (e,f) with 2 N load.