(a) The obtained response as well as recovery times for the PtAu/SnO2 sensors to acetone (10 ppm) at 300 °C. (b) Repeatability of the PtAu/SnO2 sensor to acetone (10 ppm) at 300 °C. (c) The 30-day stability tests of PtAu/SnO2 sensors against acetone (10 ppm) at 300 °C. (d) Response of PtAu/SnO2 sensor across varying relative humidities to acetone (100 ppm) at 300 °C.