Skip to main content
. 2024 Jun 27;16(13):1831. doi: 10.3390/polym16131831

Figure 14.

Figure 14

(a) Photograph of injection moulded and 3YSZ/bimodal SS 316L micro-part sintered at 1350 °C, (b) shrinkage in 3YSZ/bimodal SS 316L micro-parts at different sintering temperatures, and (c) relative density of 3YSZ/bimodal SS 316L micro-parts at different sintering temperatures.