Skip to main content
. 2024 Jun 21;10(12):e33223. doi: 10.1016/j.heliyon.2024.e33223

Fig. 13.

Fig. 13

SEM images of test specimens made of PETG coated with nHA

and PLA filament coated with nHA

(a) test specimen made of PETG filament coated with nHA: magnification 250×

(b) test specimen made of PLA filament coated with nHA: magnification 250×

(c) test specimen made of PETG filament coated with nHA: magnification 500×

(d) test specimen made of PLA filament coated with nHA: magnification 500×

▲ indicate incorporated nHA particles with sizes from 2 μm to 12.5 μm

* indicates partially incorporated nHA particles with a size of 10 μm

(e) test specimen made of PETG filament coated with nHA: magnification 1,000×

(f) test specimen made of PLA filament coated with nHA: magnification 1,000×

▲ indicate incorporated nHA particles with sizes from 2 μm to 12.5 μm

* indicates partially incorporated nHA particles with a size of 10 μm

(g) test specimen made of PETG filament coated with nHA: magnification 2,000×

▲ indicate incorporated nHA particles with sizes from 2 μm to 5 μm

* indicates partially incorporated nHA particles with a size of 10 μm

(h) test specimen made of PLA filament coated with nHA: magnification 2,000×

▲ indicate incorporated nHA particles with sizes from 2 μm to 12.5 μm

* indicates partially incorporated nHA particles with a size of 10 μm.