Skip to main content
. 2024 Jun 21;10(12):e33223. doi: 10.1016/j.heliyon.2024.e33223

Fig. 14.

Fig. 14

SEM images of test specimens made of PETG coated with nFA

and PLA filament coated with nFA

(a) test specimen made of PETG filament coated with nFA: magnification 250×

(b) test specimen made of PLA filament coated with nFA: magnification 250×

▲ point to incorporated nFA particles with a size of 5 μm

c) test specimen made of PETG filament coated with nFA: magnification 500×

d) test specimen made of PLA filament coated with nFA: magnification 500×

▲ point to incorporated nFA particles with a size of

▲ show partially incorporated, agglomerated nFA particles with a size of 5 μm

* indicates a fully incorporated nFA particle with a size of 7.5 μm m

f) test specimen made of PLA filament coated with nFA: magnification 1,000×

▲ point to incorporated nFA particles with a size of 5 μm

g) test specimen made of PETG filament coated with nFA: magnification 2,000×

▲ show partially incorporated, agglomerated nFA particles with a size of 5 μm

* indicates a fully incorporated nFA particle with a size of 7.5 μm m.