Skip to main content
. 2024 May 17;11(28):2309786. doi: 10.1002/advs.202309786

Figure 3.

Figure 3

Measured sizes of F8BT nanoparticles via dynamic light scattering (DLS) are presented: a) without crosslinker and photocrosslinked with b) CL‐C2, c) CL‐C11, and d) CL‐TEG. Insets feature liquid‐phase transmission electron microscopy (LP‐TEM) images. The samples were photocrosslinked via exposure to 365 nm UV light for 30 min.