Figure 3.

Figure 3

Surface topography of NiTi alloy in initial state on a ground surface (a), polished surface (b), and with TiO2 surface layers produced at 290 °C on ground surface (c), at 290 °C on polished surface (d), at 190 °C on ground surface (e), and at 390 °C on ground surface (f), as visualized by optical profilometer.