Skip to main content
. 2024 Jul 24;25(15):8066. doi: 10.3390/ijms25158066

Figure 3.

Figure 3

Pore size distribution and adsorption/desorption curves of bioactive glass particles for cBAG (a,b) and SrMgBAG (c,d).