Figure 3.

Figure 3

(A) SEM images for uncoated and TMS+NH3/O2 plasma-nanocoated L605 stents after 7-day immersion test in flow conditions; (B) EDS spectra of adsorbed mineral products on the stents. The TMS+NH3/O2 plasma nanocoating thickness was 20–25 nm.