Skip to main content
. 2024 Aug 5;16(15):2223. doi: 10.3390/polym16152223

Figure 15.

Figure 15

Figure 15

µ-CT cross-section of weave OS specimen after (a) 25 J, (c) 33 J impact and subsequent (b,d) repairs.