Skip to main content
. 2024 Aug 12;14(34):24815–24827. doi: 10.1039/d4ra02485k

Fig. 4. SEM test results – 10 000× magnification and distribution of fiber diameters for HA/PCL/gelatin samples with variations in the ratio of sample (A) 50 : 40 : 10 sample (B) 50 : 30 : 20 sample (C) 50 : 25 : 25 sample (D) 50 : 20 : 30 and sample (E) 50 : 35 : 15.

Fig. 4