Skip to main content
. 2024 Jun 17;11(31):2400938. doi: 10.1002/advs.202400938

Figure 2.

Figure 2

A) Shear peel curves of PBnA eutectogel prepared in DES with various [Men]:[Thy] molar ratios at 0, 20, and 40 °C. B) Tensile stress‐strain curves (left) and mechanical properties (right) of PBnA eutectogel prepared in DES with a [Men]:[Thy] molar ratio of 1:0.5. C) Tensile stress‐strain curves (left) and mechanical properties (right) of PBnA eutectogel prepared in DES with a [Men]:[Thy] molar ratio of 1:4.