Skip to main content
. 2024 Aug 6;58(33):14775–14785. doi: 10.1021/acs.est.3c09891

Figure 2.

Figure 2

SEM images of surface morphology with magnification of 250× by increasing weathering exposure days for HDPE (A,B,C,D at T0, T1, T2, and T3, respectively), LDPE (E,F,G,H at T0, T1, T2, and T3, respectively), PC (I,J,K,L at T0, T1, T2, and T3, respectively), PP (M,N,O,P at T0, T1, T2, and T3, respectively), and PS (Q,R,S,T at T0, T1, T2, and T3, respectively).