Skip to main content
. 2024 Aug 9;9(33):35888–35905. doi: 10.1021/acsomega.4c04857

Table 5. Ca/Si and Al/Si Atomic Ratios of 180 Day Cured Activated Slag Binders as a Function of the Activator Typea.

activator type Ca/Si ratio Al/Si ratio
NaOH 1.70 ± 0.30 0.31 ± 0.06
NaAc 1.21 ± 0.09 0.29 ± 0.05
KOH 1.30 ± 0.12 0.29 ± 0.04
KAc 1.21 ± 0.10 0.28 ± 0.05
a

Values correspond to the average and one standard deviation of 47 measurements conducted in the main binding phase.