Table 3. Results of Slow Constant Cooling KHI Experiments for Polymers at 2500 ppm.
| additive | concn. (ppm) | To (av.) (°C) | Ta (av.) (°C) | To – Ta (av.) (°C) |
|---|---|---|---|---|
| deionized water | 16.9 | 16.8 | 0.1 | |
| PVP | 2500 | 13.9 | 10.3 | 3.6 |
| PVCap | 2500 | 10.4 | 9.9 | 0.5 |
| Poly iC3-Me(17,20) | 2500 | 13.0 | 12.9 | 0.1 |
| Poly iC3-Et(19,20) | 2500 | 13.3 | 13.0 | 0.3 |
| Poly iC3-Pr(19,20) | 2500 | 10.4 | 10.2 | 0.2 |
| Poly-C3-Pr | 2500 | 13.2 | 11.9 | 1.3 |
| Poly-C4-Pr | 2500 | 13.2 | 12.3 | 0.9 |
| Poly-C5-Pr | 2500 | 14.6 | 12.9 | 1.7 |
| Poly iC4-Pr | 1000 | 12.3 | 11.7 | 0.6 |
| Poly iC4-Pr | 2500 | 10.4 | 9.3 | 1.1 |
| Poly iC4-Pr | 2500 + 10 000 BGE | 9.1 | 8.1 | 1.0 |