Table 2. The microtensile bond strength means (MPa), standard deviations, and distribution of the failure mode for all experimental groups.
Repair protocol | Bond strength | Mixed/Adhesive | Cohesive | Premature |
---|---|---|---|---|
SBU ER+ RC | 21.1 ± 7.7B | 34 (70.8%) | 14 (29.2%) | 0 (0%) |
SBU SE + RC | 12.0 ± 7.6B | 26 (53.1%) | 17 (34.7%) | 6 (12.2%) |
RMGIC | 33.7 ± 8.6A | 34 (50%) | 33 (48.5%) | 1 (1.5%) |
SBU: Scotchbond Universal Adhesive; ER: etch-and-rinse; SE: self-etch; RC: resin composite; RMGIC: resin-modified glass ionomer cement.*Different capital superscript letters indicate statistically significance differences between bond strength values of the repaired groups (p < 0.01).