PoS
Experimental Run Water Content (g·100 g−1) Solubility (g·100 g−1) aw
(Decimal)
WVP (g·mm/m2 day·kPa) Thickness (mm)
1 20.36 ± 7.75 17.74 ± 3.67 0.539 ± 0.013 4.39 ± 0.07 0.033 ± 0.004
2 27.06 ± 1.51 20.17 ± 1.77 0.493 ± 0.008 3.12 ± 0.17 0.032 ± 0.006
3 15.95 ± 0.92 11.48 ± 3.66 0.436 ± 0.012 4.86 ± 0.08 0.068 ± 0.017
4 10.32 ± 3.87 5.29 ± 1.06 0.429 ± 0.008 5.82 ± 0.53 0.049 ± 0.003
5 29.94 ± 3.09 16.90 ± 0.91 0.538 ± 0.006 4.33 ± 0.47 0.024 ± 0.004
6 12.11 ± 1.46 3.13 ± 0.44 0.416 ± 0.005 2.64 ± 0.26 0.057 ± 0.004
7 23.35 ± 1.38 11.90 ± 0.23 0.517 ± 0.005 6.80 ± 0.22 0.042 ± 0.002
8 19.63 ± 0.75 12.33 ± 0.16 0.518 ± 0.005 4.70 ± 0.15 0.042 ± 0.002
9 18.26 ± 3.74 15.76 ± 0.58 0.517 ± 0.007 5.78 ± 0.03 0.045 ± 0.004
10 21.62 ± 4.63 16.27 ± 2.19 0.497 ± 0.002 5.68 ± 0.56 0.045 ± 0.004
11 20.33 ± 2.15 24.04 ± 0.31 0.516 ± 0.009 6.31 ± 0.19 0.042 ± 0.002
CaS
Experimental Run Water Content (g·100 g−1) Solubility (g·100 g−1) aw
(Decimal)
WVP (g·mm/m2 day·kPa) Thickness (mm)
1 13.65 ± 1.44 9.96 ± 1.57 0.440 ± 0.006 8.02 ± 0.89 0.034 ± 0.005
2 13.26 ± 3.27 16.53 ± 1.84 0.441 ± 0.007 2.95 ± 0.27 0.030 ± 0.002
3 12.38 ± 2.11 5.41 ± 0.70 0.533 ± 0.004 3.26 ± 0.52 0.030 ± 0.005
4 15.47 ± 1.13 11.35 ± 1.64 0.529 ± 0.011 2.27 ± 0.06 0.032 ± 0.003
5 7.95 ± 1.78 10.50 ± 0.46 0.489 ± 0.011 4.42 ± 0.15 0.023 ± 0.002
6 15.03 ± 0.95 11.04 ± 0.29 0.436 ± 0.004 3.33 ± 0.66 0.057 ± 0.006
7 4.10 ± 0.73 15.73 ± 0.96 0.471 ± 0.004 3.80 ± 0.31 0.036 ± 0.008
8 6.19 ± 0.22 18.39 ± 1.77 0.464 ± 0.022 3.24 ± 0.18 0.032 ± 0.004
9 10.21 ± 1.52 5.44 ± 2.77 0.457 ± 0.011 2.42 ± 0.18 0.024 ± 0.000
10 11.45 ± 0.61 3.39 ± 0.25 0.429 ± 0.008 2.42 ± 0.19 0.032 ± 0.002
11 11.40 ± 0.72 3.06 ± 0.46 0.447 ± 0.005 2.40 ± 0.59 0.034 ± 0.003