Skip to main content
. 2024 Sep 11;42:519–530. doi: 10.1016/j.bioactmat.2024.08.048

Fig. 2.

Fig. 2

(a) Mg alloy scaffold infiltrated with α-TCP paste (L/P = 0.50 ml/g), (b–d) detail of the conformation of the α-TCP paste to the porosity and surface of the scaffolds, (e) composite after 24 h of immersion in water at 37 °C, (f) surface and (g) cross-section at 45° of the composite after 30 min of incubation in an autoclave at 190 °C. (a, e, f) digital camera, (b–d, g) LM, and (c, d) 3D view.