Skip to main content
. 2024 Sep 18;17(18):4579. doi: 10.3390/ma17184579

Figure 12.

Figure 12

The comparison of the specific mass gain tested at 1000 °C for 20 h among NbTi-bearing RMEAs and RHEAs from this work, AlCrMo + Nb/NbTi/TaTi [25], CrNbTiZr [28] and AlHfMoNbTi [38] from the literature.