The rheological properties of Alginate+Hyaluronan‐Tyramine (AHAT) and Hyaluronan‐Tyramine (HAT) inks (n = 6) performed at 21 °C

Ink Storage Modulus [G’] Loss Modulus [G’’] tan δ Yield Stress [Pa] K [Pa sn] n R 2
AHAT (1% A; 2.5% HAT) 203 ± 13 23.6 ± 3 0.116 574 ± 22 2467 0.2683 0.9995