. 2024 Sep 23;4(10):2573–2584. doi: 10.1021/acsestengg.4c00317

Table 2. Summary of Electrode Alteration and Operational Performance.

  Electrode porosity
Parameter Nonporous (solid) Low (10 PPI) Intermediate (50 PPI) High (100 PPI)
Anode alteration Evident pitting corrosion Evident pitting corrosion Evident pitting corrosion Severe internal pore clogging
Slight surface deposition No pore clogging Moderate surface deposition Moderate surface deposition
  Structural instability    
  Uniform usage of outer and inner pores. Insignificant pore clogging Moderate pore clogging
Cathode alteration Slight surface deposition Severe surface deposition Moderate surface coverage Severe surface coverage
  No pore clogging Insignificant internal pore clogging Severe internal pore clogging
Faradaic efficiency of iron dosing As predicted (∼100%) Super-Faradaic (>100%) As predicted (∼100%) Sub-Faradaic (<100%)
Energy consumption Moderate High Low Low
Overall performance Moderate Poor Best Moderate