. 2024 Sep 30;16(19):2786. doi: 10.3390/polym16192786

Figure 11.

Figure 11

Figure 11

The DSC heating thermograms of the first (solid line), second (dashed line), and third (dotted line) heating runs for the polymers P1 (A), P2 (B), P3 (C), P4 (D), P5 (E), and P6 (F). The heating rate β = 5 °C min−1 in a nitrogen atmosphere at 50 mL·min−1.