Glass transition temperatures (Tg) and changes in heat capacity (ΔCp) of G3 eutectic mixture with varying water content (0%, 5%, 10%, 15%, 20%, and 25%), during the first heating and cooling cycles.

Sample Code First Heating First Cooling
Ton (°C) Tg (°C) ΔC
J/(g·°C)
Ton (°C) Tg (°C) ΔC
J/(g·°C)
G3-0 −74.5 ± 0.7 −68.3 ± 0.5 0.65 ± 0.03 −58.4 ± 0.5 −68.3 ± 0.3 0.68 ± 0.03
G3-5 −68.4 ± 0.6 −60.6 ± 0.4 0.59 ± 0.02 −52.2 ± 0.4 −61.4 ± 0.2 0.60 ± 0.02
G3-10 −67.6 ± 0.6 −59.9 ± 0.2 0.64 ± 0.02 −49.2 ± 0.5 −62.1 ± 0.3 0.70 ± 0.02
G3-15 −65.4 ± 0.5 −57.2 ± 0.2 0.64 ± 0.02 −50.5 ± 0.5 −60.5 ± 0.3 0.63 ± 0.01
G3-20 −70.0 ± 0.4 −62.7 ± 0.3 0.61 ± 0.01 −51.3 ± 0.4 −59.8 ± 0.2 0.62 ± 0.02
G3-25 −63.5 ± 0.7 −55.1 ± 0.5 0.61 ± 0.02 −44.6 ± 0.4 −58.1 ± 0.2 0.59 ± 0.02