Skip to main content
. 2024 Oct 28;14(46):34239–34252. doi: 10.1039/d4ra07469f

Fig. 13. LP diagram of X-scratched samples (a) pristine nickel coating, (b) self-healing coating with 10 g L−1 microcapsules, (c) self-healing coating with 20 g L−1 microcapsules, (d) self-healing coating with 30 g L−1 microcapsules, in the bath and (e) mild steel substrate without coating.