Skip to main content
. 2024 Oct 18;40(43):22762–22772. doi: 10.1021/acs.langmuir.4c02753

Figure 4.

Figure 4

TEM images of encapsulated SPs. The images were taken after magnetic purification and reveal an increasing polymer shell thickness with increasing volume of the added styrene/DVB mixture (140, 200, and 280 μL). The TGA data (lower left panel) confirm an increasing organic fraction of the encapsulated SPs with increasing volume of added monomers.